Send Message
Danyang Kaixin Alloy Material Co., Ltd.
Products
Products
Home > Products > Expansion Alloy > 4J52 Expansion Alloy Corrosion Resistant Alloy Light Rod

4J52 Expansion Alloy Corrosion Resistant Alloy Light Rod

Product Details

Place of Origin: China

Brand Name: KAIXIN

Certification: ISO9001:2015

Model Number: KX-Alloy EX50

Payment & Shipping Terms

Minimum Order Quantity: 200KG

Price: To negotiate

Packaging Details: Wooden Box, size as per guests's request

Delivery Time: 45~60days

Payment Terms: T/T, L/C

Supply Ability: 50~80TONS per MONTH

Get Best Price
Highlight:

4J52 Expansion Alloy

,

Expansion Alloy ASTM

,

High strength corrosion resistant alloy

Features:
High Strength And Corrosion Resistance
Shape:
Wire,Strip,Rod,Tube,Plate
Alloy Type:
Fe-Ni Constant Expansion Alloy
Raw Materials:
NI51.5-52.5%,Fe Rem
Executive Standard:
ASTM
Delivery State:
Soft State
Application:
For Aerospace, Nuclear Energy, Petroleum Industry, Electric Vacuum Industry, Soft Glass Or Ceramic Matching Sealing.
Size:
Negotiable
Features:
High Strength And Corrosion Resistance
Shape:
Wire,Strip,Rod,Tube,Plate
Alloy Type:
Fe-Ni Constant Expansion Alloy
Raw Materials:
NI51.5-52.5%,Fe Rem
Executive Standard:
ASTM
Delivery State:
Soft State
Application:
For Aerospace, Nuclear Energy, Petroleum Industry, Electric Vacuum Industry, Soft Glass Or Ceramic Matching Sealing.
Size:
Negotiable
4J52 Expansion Alloy Corrosion Resistant Alloy Light Rod

KX 4J52 Corrosion Resistant Alloy Light Rod On Expansion Alloy

 

Product Description and Application

 

4J52 is something like Alloy 50

4J52 has excellent comprehensive properties in the temperature range from -253 ℃ to 700℃. The yield strength below 650℃ ranks the first among deformed superalloys, and has excellent performance, machining performance and welding performance. It can manufacture all kinds of parts with complex shapes, and has been widely used in aerospace, nuclear energy, petroleum industry and extrusion mold in the above temperature range.

 

 

Process Performance and Requirements

 

  • Product Fusion Process

 

Vacuum Induction Furnace(VIM) and Electroslag Remelting Furnace(ESR)

 

  • Product Chemical Composition 

 

Alloy Grade C P S Mn Si Al Co Ni Fe
Not more than  
4J52 0.05 0.02 0.02 0.6 0.3 ---- --- 51.5~ 52.5 Rem

 

  • Product Mechanical Property

 

WireTensile Strength 

State Code State Tensile strength/MPa
R Soft State <590
I Hard State >820

 

Strip Tensile Strength 

State Code State

Tensile strength

/MPa

R Soft State <570
I Hard State >700

 

  • Product Average Coefficient of Linear Expansion

 

Alloy Grade Sample Heat Treatment Institution

Average Coefficient of Linear Expansion

α/(10-6/ K)

20~ 300℃ 20~ 400 ℃ 20~ 450 ℃
4J52 It is heated to 850±20 in hydrogen atmosphere, heat preservation for 1 hour and cool to less than 200 at a speed of no more than 5 / min 9.8~ 11.0 9.81~ 11.0  

 

 

  • Product Melting Temperature Range

 

Melting Temperature 1430℃
Thermal Conductivity λ=16.7W/(m·℃)[1,2]
Specific Heat Capacity 502J/(kg/℃)

 

 

  • Productive Process

 

4J52 Expansion Alloy Corrosion Resistant Alloy Light Rod 0

 

 

 

  • Professional Customization

Cold-drawn Wire ¢0.3~¢18mm(Delivery in rolls or trays)
Hot-Rolling Wire ¢5.5~¢20mm(Delivery in rolls)
Strip thickness 0.1~4.5*width 6~350mm(Supply in rolls or straight strips)
Smooth Forged Rod on a Lathe

¢60~350mm,L800-2500mm

Hot-rolled Burnishing ¢20~80mm,L1000-5000mm
Cold Drawn and Burnishing ¢2.5~18mm,L1000-8000mm
Seamless Tube ¢1~275mm,wall thickness 0.2~30,L1000-8000mm

 

4J52 Expansion Alloy Corrosion Resistant Alloy Light Rod 1

 

4J52 Expansion Alloy Corrosion Resistant Alloy Light Rod 24J52 Expansion Alloy Corrosion Resistant Alloy Light Rod 34J52 Expansion Alloy Corrosion Resistant Alloy Light Rod 44J52 Expansion Alloy Corrosion Resistant Alloy Light Rod 5