No6625 Welding Rod Alloy 625 TIG Nickel Chromium Based Superalloy

Product Details

Place of Origin: China

Brand Name: KAIXIN

Certification: ISO9001:2015

Model Number: KA-ALLOY no6625

Payment & Shipping Terms

Minimum Order Quantity: 30kg

Price: 38-40 USD/kg

Packaging Details: Wooden Box, size as per guests request

Delivery Time: 15-20 DAYS

Supply Ability: 10000KG/MONTH

Get Best Price
Highlight:

No6625 Welding Rod

,

Alloy 625 TIG

,

Nickel Chromium Based Superalloy

Corrosion Resistance:
Excellent
Density:
8.2 G/cm3
Elongation:
Up To 40%
Formability:
Good
Hardness:
Up To 40 HRC
Material:
Inconel Alloy
Melting Point:
1350-1400°C (2460-2550°F)
Modulus Of Elasticity:
200 GPa (29 X 10 6 Psi)
Tensile Strength:
Up To 1,400 MPa (200,000 Psi)
Thermal Conductivity:
25 W/mK (100 BTU In/hr Ft² °F)
Thermal Expansion:
13.3 μm/m°C (7.3 X 10-6 In/in°F)
Type:
Nickel-Chromium-Based Superalloy
Name:
No6625 /Alloy 625 TIG
Corrosion Resistance:
Excellent
Density:
8.2 G/cm3
Elongation:
Up To 40%
Formability:
Good
Hardness:
Up To 40 HRC
Material:
Inconel Alloy
Melting Point:
1350-1400°C (2460-2550°F)
Modulus Of Elasticity:
200 GPa (29 X 10 6 Psi)
Tensile Strength:
Up To 1,400 MPa (200,000 Psi)
Thermal Conductivity:
25 W/mK (100 BTU In/hr Ft² °F)
Thermal Expansion:
13.3 μm/m°C (7.3 X 10-6 In/in°F)
Type:
Nickel-Chromium-Based Superalloy
Name:
No6625 /Alloy 625 TIG
No6625 Welding Rod Alloy 625 TIG Nickel Chromium Based Superalloy

Good Price And High Quality No6625 Welding Rod Factory Direct Supply ( Alloy 625 TIG)

No6625  Product Fusion Process

Vacuum Induction Furnace(VIM) and Electroslag Remelting Furnace(ESR)
Product Chemical Composition
 
      Grade
%
Ni
Cr
Mo
Nb
Fe
Al
Ti
No6625
Min
Rem
20
8
3.15
 
 
 
Max
 
23
10
4.15
5
0.4
0.4
   Grade
%
C
Mn
Si
Co
P
S
 
No6625
Min
 
 
 
 
 
 
 
Max
0.1
0.5
0.5
1
0.015
0.015
 

 

Product Physical Property
Density
8.44kg/m3
Melting point
1290-1350℃
Magnetic Property
Nil

No6625 is a nickel-chromium-molybdenum alloy that has been specifically designed to possess high strength, corrosion resistance, and oxidation resistance. One of the key features of Inconel 625 is its ability to withstand high temperatures and withstand long-term creep under heavy loads.
No6625 has a microstructure that consists of a combination of intermetallic phases and interdiffused metal phases. These microstructural features contribute to the alloy's strength and resistance to corrosion.
One of the key microstructural features of UNS N06625 is the formation of phase precipitates. These precipitates are composed of Ni3(Nb, Al, Ti) and have a tetragonal crystal structure. The γ” phase precipitates are ordered A3 B type, meaning they have a particular arrangement of atoms.
These γ” phase precipitates are coherent with respect to the matrix, meaning they form a disk-shaped morphology and are stable at high temperatures. However, there are also some γ” phase precipitates that have a needle-like morphology and are not coherent with the matrix.
The formation of these γ” phase precipitates is important for the material's ability to recover creep properties. When subjected to long-term creep under heavy loads, the γ” phase precipitates can recover some of the alloy's strength and elongation, thereby prolonging the material's lifetime.
Overall, the combination of the microstructure and γ” phase precipitates of No6625 contribute to its exceptional performance in high-temperature and high-load environments.

 

Pipe Seamless Pipe Welded Tube Seamless Tube Welded Sheet/Plate Bar Forging Fitting welding Wire
B444 B705 B444 B704 B443 B446 – – AWS 5.14:2018

 

No6625  W.Nr. 2.4856 ,UNS NO6625,Nickel Alloy 625,Inconel 625

Markets

 

Markets for No6625 include:

  • Offshore
  • Marine
  • Nuclear
  • Chemical Processing
  • Aerospace
  • Glow Plugs

Applications

Product and technology applications of No6625 include:

  • Seawater components
  • Flare stacks
  • Aircraft ducting systems
  • Fabrication with No6625
  • Specialized seawater equipment
  • Chemical process equipment
  • Turbine shroud rings
  • Engine thrust-reverser systems
  • Jet engine exhausts systems
  • Boiler furnaces

No6625 Welding Rod Alloy 625 TIG Nickel Chromium Based SuperalloyNo6625 Welding Rod Alloy 625 TIG Nickel Chromium Based Superalloy